Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AKROMID® B3 1 FR black (6580) - PA6 - Akro-Plastic GmbH

Material Data Center offers the following functions for AKROMID® B3 1 FR black (6580):
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Akromid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
성형 수축률, 평행 1.0 / * % ISO 294-4, 2577
성형 수축률, 수직 1.1 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 3600 / 1300 MPa ISO 527
항복강도 75 / 40 MPa ISO 527
굴곡 계수, 23°C 3500 / 1300 MPa ISO 178
굴곡 강도 115 / 45 MPa ISO 178
챠피 충격 강도, +23°C 78 / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 4.5 / 13 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 220 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 60 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 180 / * °C ISO 75-1/-2
선형 열팽창 계수, 평행 78 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 78 / * E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 V-0 / * class IEC 60695-11-10
테스트 두께 1.6 / * mm -
Yellow Card 유효한 예 / * - -
두께 H인 제품의 난연성 V-0 / * class IEC 60695-11-10
테스트 두께 0.4 / * mm -
Yellow Card 유효한 예 / * - -
두께가 h인 제품의 난연성 등급 5V 5VA / * class IEC 60695-11-20
테스트 두께 3.2 / * mm -
산소지수로서의 난연성 32 / * % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.4 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 0.8 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 1.6 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.4 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (2) 0.8 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (3) 1.6 mm -
전기적 특성건조/응축단위시험규격
ISO 데이터
전기 압력 10 / - kV/mm IEC 60243-1
CTI 600 / - - IEC 60112
기타 특성건조/응축단위시험규격
밀도 1190 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
용융수지온도 270 °C -
성형온도 80 °C -
Injection pressure 75 MPa -
도표
점도-변형률 , AKROMID® B3 1 FR black (6580), PA6, Akro-Plastic
전단-변형률 , AKROMID® B3 1 FR black (6580), PA6, Akro-Plastic
비용적-온도(pvT) , AKROMID® B3 1 FR black (6580), PA6, Akro-Plastic
특징
생산 공정
사출 성형
인도 유형
검정
특별 특성
난연성, Halogen-free, 열안정성
Certifications
RoHS
응용
전기 및 전자
지역별 검색
짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com